Abstract
The mechanical properties and fracture mode of 60Co γ-ray irradiated blends of plasticized poly(vinyl chloride) [PVC] and thermoplastic copolyester elastomer [Hytrel 40D] have been investigated with specific reference to the effect of blend ratios and absorbed radiation doses. Samples were irradiated in the dose range of 0.1-50 Mrad in air at room temperature (25°C) at the rate of 0.321 Mrad/h. Hytrel and blends containing higher proportion of hytrel (≥50%) were found to undergo extensive crosslinking in the bulk which in effect caused a maximum in ultimate tensile strength at an absorbed dose of 1 Mrad, but showed a drastic drop in tensile strength at higher radiation doses (10-50 Mrad) due to embrittlement and surface oxidation. In the case of PVC and blends containing a higher proportion of PVC (≥75%), a slow decline in tensile strength was observed at lower radiation doses up to 10 Mrad, whereas at higher doses (10-50 Mrad), they showed a sharp decrease in tensile strength due to the degradation of the PVC phase. The elongation at break, tear strength and tensile set after failure of all the samples remain unchanged up to an absorbed dose of 1 Mrad but showed considerable reduction at higher radiation doses. The morphology of the irradiated surfaces after an absorbed dose of 50 Mrad has been examined by scanning electron microscope (SEM). SEM studies on the tensile and tear fracture surfaces also have been undertaken in order to gain an insight into the mechanism of failure.
| Original language | English |
|---|---|
| Pages (from-to) | 283-294 |
| Number of pages | 12 |
| Journal | International Journal of Radiation Applications and Instrumentation. Part |
| Volume | 28 |
| Issue number | 3 |
| DOIs | |
| Publication status | Published - 1986 |
| Externally published | Yes |
Fingerprint
Dive into the research topics of 'Studies on mechanical properties and fractography of γ-ray irradiated blends of plasticized poly(vinyl chloride) and thermoplastic copolyester elastomer'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver