Skip to main navigation Skip to search Skip to main content

Improving atomic layer deposition process through reactor scale simulation

  • University of Wisconsin
  • University of Alaska Anchorage

Research output: Contribution to journalArticlepeer-review

28 Citations (Scopus)

Abstract

In order to modify atomic layer deposition (ALD) characteristics of Al 2O3, three-dimensional gas transports and film depositions are investigated through reactor scale simulations inside two different viscous flow reactors. In the top-inlet reactor (TIR), the gaseous species are directly injected into the substrates from the upper surface of the reactor while in the bottom-inlet reactor (BIR), the inlet is at the bottom of the reactor and next to the substrate. The numerical procedure to simulate the ALD process is thoroughly explained by using the multi-species and multi-reaction chemistry phenomena. The reactants are trimethylaluminum (TMA) and ozone, and the simulations are performed in an operating pressure of 10 Torr (1330 Pa) and two substrate temperatures of 250 °C and 300°C. Due to the chemistry mechanism used in this study, a long ozone exposure is a crucial parameter to deliver a sufficiently oxidized substrate. For a specific reactor type, deposition rates are higher on the hotter substrate due to both a larger surface reaction rate constant and greater concentrations of the oxygen atoms on the substrate. At a fixed substrate temperature, higher deposition rates are obtained by using the TIR. The same deposition rate distributions are obtained among all cycles for each ALD process that result in the dependency of the film thickness only on the numbers of ALD cycles. For the substrate at 250 °C, the growth rates are equal to 3.78 Å/cycle and 4.43 Å/cycle in the BIR and the TIR, respectively, and for the substrate at 300 °C, the growth rates are equal to 4.52 Å/cycle and 6.49 Å/cycle in the BIR and the TIR, respectively.

Original languageEnglish
Pages (from-to)1243-1253
Number of pages11
JournalInternational Journal of Heat and Mass Transfer
Volume78
DOIs
Publication statusPublished - Nov 2014
Externally publishedYes

Keywords

  • Atomic layer deposition
  • Gas-phase reaction
  • Mass deposition rate
  • Navier-Stokes equation
  • Surface reaction
  • Viscous flow reactor

ASJC Scopus subject areas

  • Condensed Matter Physics
  • Mechanical Engineering
  • Fluid Flow and Transfer Processes

Fingerprint

Dive into the research topics of 'Improving atomic layer deposition process through reactor scale simulation'. Together they form a unique fingerprint.

Cite this